The table below shows four welding defects - NSC Agricultural Technology - Question 4 - 2021 - Paper 1
Question 4
The table below shows four welding defects. Redraw the table in your ANSWER BOOK and write down the answers to QUESTIONS 4.1.1 to 4.1.8.
| Illustration | Name of th... show full transcript
Worked Solution & Example Answer:The table below shows four welding defects - NSC Agricultural Technology - Question 4 - 2021 - Paper 1
Step 1
4.1.1 Name of the Welding Defect
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The defects illustrated are:
Porosity
Spatter
Undercut
Lack of fusion