Step 1

4.1.1 Name of Welding Defect

96%

114 rated

Answer

Porosity

Step 2

4.1.2 Give the Possible Causes

99%

104 rated

Answer

Blocked nozzle, gas flow too low or too high, welding arc length is too long, moisture in the weld area.

Step 3

4.1.3 Name of Welding Defect

96%

101 rated

Answer

Spatter

Step 4

4.1.4 Give the Possible Causes

98%

120 rated

Answer

Voltage too low, inadequate surface preparation, rusty or dirty metal.

Step 5

4.1.5 Name of Welding Defect

97%

117 rated

Answer

Undercut

Step 6

4.1.6 Give the Possible Causes

97%

121 rated

Answer

Welding speed too fast, incorrect travel angle.

Step 7

4.1.7 Name of Welding Defect

96%

114 rated

Answer

Lack of fusion

Step 8

4.1.8 Give the Possible Causes

99%

104 rated

Answer

Amperage too low, wrong torch angle.