The table below shows four welding defects - NSC Agricultural Technology - Question 4 - 2021 - Paper 1
Question 4
The table below shows four welding defects. Redraw the table in your ANSWER BOOK and write down the answers to QUESTIONS 4.1.1 to 4.1.8.
| Illustration | Name of th... show full transcript
Worked Solution & Example Answer:The table below shows four welding defects - NSC Agricultural Technology - Question 4 - 2021 - Paper 1
Step 1
4.1.1 Name of the Welding Defect
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Porosity
Step 2
4.1.2 Possible Causes
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
• Blocked nozzle
• Gas flow too low or high
• Irregular gas mix
• Undercutting due to improper torch angle
• Plate not cleaned properly
Step 3
4.1.3 Name of the Welding Defect
96%
101 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Spatter
Step 4
4.1.4 Possible Causes
98%
120 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
• Voltage too low
• Inductance too low
• Rusty or dirty surface
Step 5
4.1.5 Name of the Welding Defect
97%
117 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Undercut
Step 6
4.1.6 Possible Causes
97%
121 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
• Welding speed too fast
• Incorrect torch angle
• Poor technique
Step 7
4.1.7 Name of the Welding Defect
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Lack of fusion
Step 8
4.1.8 Possible Causes
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!