6.1 What welding defect is described as non-metallic solids trapped in the weld metal?
6.2 Name FOUR defects that may be observed during visual inspections - NSC Mechanical Technology Automotive - Question 6 - 2017 - Paper 1
Question 6
6.1 What welding defect is described as non-metallic solids trapped in the weld metal?
6.2 Name FOUR defects that may be observed during visual inspections.
6.3 St... show full transcript
Worked Solution & Example Answer:6.1 What welding defect is described as non-metallic solids trapped in the weld metal?
6.2 Name FOUR defects that may be observed during visual inspections - NSC Mechanical Technology Automotive - Question 6 - 2017 - Paper 1
Step 1
What welding defect is described as non-metallic solids trapped in the weld metal?
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The welding defect described is called slag inclusion. This defect occurs when non-metallic materials become trapped in the weld metal, compromising the integrity of the weld.
Step 2
Name FOUR defects that may be observed during visual inspections.
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
During visual inspections, the following defects may be observed:
Shape of profile: Irregularities in the geometric shape of the weld.
Uniformity of surface: Variability in the surface texture and appearance of the weld.
Overlap: Metal not properly fused to the base material, leading to a protruding weld.
Crack free: Identifying surface cracks that may indicate weakness in the weld.
Step 3
State TWO causes of incomplete penetration in a welded joint.
96%
101 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Two common causes of incomplete penetration in a welded joint are:
Weld speed too fast: This can prevent sufficient heat from being generated to penetrate the base metal adequately.
Electrode too large: Using an electrode that is too large may result in insufficient melting of the base material, leading to incomplete penetration.
Step 4
Name TWO measures to prevent a lack of fusion in a welded joint.
98%
120 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
To prevent a lack of fusion in a welded joint, the following measures can be implemented:
Correct preparation of joint: Ensuring that the surfaces to be welded are properly cleaned and aligned can enhance fusion.
Correct weld speed: Maintaining an appropriate speed during the welding process helps achieve good fusion between the weld metal and base metal.
Step 5
To determine the weld hardness and strength
97%
117 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The test used to determine the weld hardness and strength is the machinability test. This test assesses how easily the welded material can be machined and provides insight into the hardness and general properties of the weld.
Step 6
To reveal internal defects
97%
121 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The test used to reveal internal defects is the nick-break test. This technique involves breaking the welded joint to visually inspect for internal flaws or weaknesses.
Step 7
To determine the ductility of the deposit and the heat-affected area adjacent to the weld
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The bend test is conducted to evaluate the ductility of the weld deposit and the heat-affected zone. This test involves bending the welded joint to assess its ability to withstand deformation without breaking.
Step 8
Explain how you will conduct a dye penetration test on a welded joint.
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
To conduct a dye penetration test on a welded joint, follow these steps:
Clean the weld: Ensure that the weld area is clean from contaminants like oil, grease, and dirt.
Apply the dye: Spray a penetrant dye onto the weld and allow it to seep into any surface cracks or defects.
Cleanup: After a specified time, clean the excess dye from the surface using a suitable cleaner.
Developer application: Apply a developer to the weld surface to make defects visible. The dye trapped in any cracks will appear against the contrasting background, highlighting any flaws.
Step 9
State ONE function of EACH of the following components on the MIG/MAGS welding equipment: Wire feed controller
96%
101 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The wire feed controller is responsible for feeding the consumable electrode wire to the welding gun at a constant predetermined speed, which is crucial for maintaining a stable arc during the welding process.
Step 10
State ONE function of EACH of the following components on the MIG/MAGS welding equipment: Welding gun
98%
120 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The welding gun activates the supply of gas, power, and wire feed to facilitate the welding process. It also provides the mechanism for directing the welding arc and ensuring efficient welding operations.
Step 11
What is the function of the inert gas used during the MIG/MAGS welding process?
97%
117 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The function of the inert gas used during the MIG/MAGS welding process is to shield the molten pool from atmospheric gases. This prevents contamination and oxidation, which can adversely affect the quality and properties of the weld.