6.1 State ONE cause of EACH of the following welding defects:
6.1.1 Porosity
6.1.2 Undercutting
6.1.3 Slag inclusion
6.2 Name THREE destructive tests that can be executed onto a welded joint - NSC Mechanical Technology Fitting and Machining - Question 6 - 2018 - Paper 1
Question 6
6.1 State ONE cause of EACH of the following welding defects:
6.1.1 Porosity
6.1.2 Undercutting
6.1.3 Slag inclusion
6.2 Name THREE destructive tests that can be ex... show full transcript
Worked Solution & Example Answer:6.1 State ONE cause of EACH of the following welding defects:
6.1.1 Porosity
6.1.2 Undercutting
6.1.3 Slag inclusion
6.2 Name THREE destructive tests that can be executed onto a welded joint - NSC Mechanical Technology Fitting and Machining - Question 6 - 2018 - Paper 1
Step 1
State ONE cause of EACH of the following welding defects: 6.1.1 Porosity
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
A primary cause of porosity during welding can be atmospheric contamination, which leads to gas pockets being trapped in the weld.
Step 2
State ONE cause of EACH of the following welding defects: 6.1.2 Undercutting
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Undercutting is often attributed to improper settings of equipment, which can cause excessive melting of the base metal.
Step 3
State ONE cause of EACH of the following welding defects: 6.1.3 Slag inclusion
96%
101 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Slag inclusion commonly occurs due to the failure to remove previous weld slag, resulting in impurities being trapped in the weld.
Step 4
Name THREE destructive tests that can be executed onto a welded joint.
98%
120 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Three destructive tests that can be performed on a welded joint include:
Nick break test
Bend test
Tensile test
Step 5
Describe how the dye penetration test is done on a welded joint.
97%
117 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The dye penetration test involves several steps:
Clean the weld: Ensure the joint is free from contaminants.
Apply dye: Spray a dye onto the surface that needs to be tested to allow it to penetrate.
Remove excess dye: Clean the surface with a cleaning agent to remove excess dye.
Allow surface to dry: Let the surface dry fully to see the results clearly.
Develop the surface: Apply a developer to bring out the dye trapped in any cracks.
Inspect: The dye will highlight all surface defects, indicating any flaws.
Step 6
What is the purpose of the inert gas used during the MIG/MAGS welding process?
97%
121 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The inert gas serves multiple purposes:
It stabilizes the arc, ensuring a steady and focused welding process.
It prevents atmospheric contamination by shielding the weld area from airborne impurities.
It minimizes weld spatter, leading to cleaner welds.
It promotes proper fusion of the materials being joined.
Step 7
State THREE factors that should be considered during the MIG/MAGS welding process.
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Three critical factors to consider during MIG/MAGS welding include:
Amount of penetration and fusion required for optimal weld strength.
The rate of wire feed to maintain consistent welding speed and quality.
The sound of the welding process, which can indicate the stability and quality of the arc.
Step 8
LABEL A to G in FIGURE 6.6
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
A: Parent metal / Work piece
B: Electrode wire
C: Gas shroud
D: Contact tube
E: Shielding gas
F: Earth cable / terminal / ground wire / skelm
G: Work piece / welded joint