8.1 State THREE welding aspects that must be focused on during the arc welding procedure - NSC Mechanical Technology Welding and Metalwork - Question 8 - 2021 - Paper 1
Question 8
8.1 State THREE welding aspects that must be focused on during the arc welding procedure.
8.2 How can centre-line cracks in welding joints be reduced?
8.3 State TW... show full transcript
Worked Solution & Example Answer:8.1 State THREE welding aspects that must be focused on during the arc welding procedure - NSC Mechanical Technology Welding and Metalwork - Question 8 - 2021 - Paper 1
Step 1
State THREE welding aspects that must be focused on during the arc welding procedure.
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Rate of rod burning and the progress of the weld.
Observe for welding defects while welding.
Correct current settings for the particular electrode.
Step 2
How can centre-line cracks in welding joints be reduced?
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Aiming at a width to depth ratio of 1:1.
Decreasing the welding current to prevent excess penetration.
Step 3
State TWO causes of EACH of the following arc-welding defects:
96%
101 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
8.3.1 Lack of fusion:
Travel speed is too slow.
Weld joint is wide.
8.3.2 Porosity:
Contaminated weld surface.
Wet or dirty electrodes.
8.3.3 Incomplete penetration:
Welding current too low.
Electrode too big.
Step 4
Describe the process of setting an oxy-acetylene torch flame to a neutral flame.
98%
120 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Open the acetylene torch valve ¼ turns or less and ignite.
Adjust the acetylene torch valve until the black smoke disappears.
Open the oxygen torch valve until the flame is no longer burning yellow.
Step 5
Explain how to conduct a guided bend test on a welded joint.
97%
117 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Specimen is placed across the supports of the die.
Apply force to the specimen to bend into the shape of the die.
Determine the percentage of elongation of the welded metal.
Step 6
State TWO aspects that are tested when conducting a free-bend test on a welded joint.
97%
121 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Determine the ductility of the weld.
Determine the percentage of elongation of the weld metal.
Step 7
Name TWO different types of dye used to conduct a liquid dye penetration test.
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Type A: Fluorescent that emits visible light when viewed using a black light.
Type B: Brightly colored liquid dyes that can be inspected in regular light.
Step 8
Explain why a nick-break test is conducted on a welded joint.
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
The nick-break test determines internal quality of the weld and reveals internal defects such as slag inclusions, porosity, and lack of fusion.