FIGUUR 6.1 toon sweistoerustingkomponente - NSC Mechanical Technology Welding and Metalwork - Question 6 - 2016 - Paper 1
Question 6
FIGUUR 6.1 toon sweistoerustingkomponente. Beantwoord die vrae wat volg.
6.1.1 Identifiseer die tipe toerusting wat in FIGUUR 6.1 getoon word.
6.1.2 Benoem kompone... show full transcript
Worked Solution & Example Answer:FIGUUR 6.1 toon sweistoerustingkomponente - NSC Mechanical Technology Welding and Metalwork - Question 6 - 2016 - Paper 1
Step 1
6.1.1 Identifiseer die tipe toerusting wat in FIGUUR 6.1 getoon word.
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Die tipe toerusting wat in FIGUUR 6.1 getoon word, is 'n MIG/MAGS-sweistoerusting.
Step 2
6.1.2 Benoem komponente A–G.
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Die komponente is soos volg:
A - Skermgasbottel
B - Reguleerder
C - Gasvloei-meter
D - Ononderbreekte draadkontrol
E - Sweispistool
F - Boog
G - Aardklamp
Step 3
6.1.3 Wat is die doel van die gas gedurende die sweisproses?
96%
101 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Die doel van die gas is om te voorkom dat suurstof met die gesmelte metaal in aanraking kom. Dit help om 'n skoon en sterk las te vorm.
Step 4
6.2.1 Noem TWEE oorsake van die defek: Slakinisolering.
98%
120 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Twee oorsake van slakinisolering is:
Ingeslote hoeke is te klein.
Vinnige afkoeling.
Step 5
6.2.2 Noem TWEE oorsake van die defek: Insnyding.
97%
117 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Twee oorsake van insnyding is:
Foutiewe elektrode-manipulasie.
Sweisproses te vinnig.
Step 6
6.3.1 Noem TWEE maatreëls om die defek: Gebrekkige smelting te voorkom.
97%
121 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Twee maatreëls om gebrekkige smelting te voorkom is:
Pas die elektrode aan en berei die V-groef behoorlik voor.
Weefsel moet voldoende wees om die kante van die las te smelt.
Step 7
6.3.2 Noem TWEE maatreëls om die defek: Sweiskraters te voorkom.
96%
114 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Twee maatreëls om sweiskraters te voorkom is:
Gebruik laer stroom.
Gebruik behoorlike sweisgeniek.
Step 8
6.4 Verduidelik hoe jy 'n kleurfoutdifferingstoets op 'n sweislas kan uitvoer.
99%
104 rated
Only available for registered users.
Sign up now to view full answer, or log in if you already have an account!
Answer
Om 'n kleurfoutdifferingstoets uit te voer:
Maak die oppervlak plat en skoon, gebruik 'n skoneretteer om enige vuilheid of oorskot te verwyder.
Kleurstof word op die oppervlak aangebring en laat dit vir 'n tyd op die oppervlak sit om te absorbeer.
Spoel die oppervlak met water en kyk vir enige kleurverandering wat dui op 'n onregte las.